FV9600 Fluorosilicone

Iki gicuruzwa gifite flame retardancy, yujuje urwego rwa UL94 / FV 0. Kurwanya amavuta meza cyane, kurwanya ibishishwa, guhangana nubushyuhe bwo hejuru kandi buke
  • FV9600

  • Herchy

Kuboneka:
Ubwinshi:

Ibipimo bya tekiniki

Ibintu

Ironderero

Icyiciro

FV9660

FV9670

Kugaragara

Uburyo bwo Kwipimisha

Cyera

Uburemere bwihariye / g / cm3

ASTM D792

1.46

1.48

Gukomera / inkombeA

ASTM D2240

60

70

Imbaraga za Tensile / MPa

ASTM D412

6.8

6.5

Kurambura Kuruhuka /%

ASTM D412

310

290

Imbaraga zamarira / KN / m

ASTM D624-B

17

17

* Kurwanya Ubushyuhe
200 ℃ × 72h

Guhinduka gukomeye / inkombe A.

+5

+5

Imbaraga zingirakamaro zihinduka,%

3.8

3.5

Imbaraga zingirakamaro zihinduka,%

161

154

IRM903
Guhindura amajwi /%
150 ℃ / 72h

ASTM D471

5.5

5.2

Ibicanwa C
Igipimo cyimpinduka /%
23 ℃ / 72h

ASTM D471

20

20

Urwego rwumuriro

GBT10707-2008

FV 0

FV 0

Gukiza

Ongeramo ibice 0.7 bya bis (2 + 5), icyiciro kimwe cya volcanisation 170 ℃ × 15min, ibirunga bibiri: 200 ℃ × 4h.


Ibyifuzo byo gutunganya


Koresha 0,6 kugeza 1 igice bis-dipenta volcanising agent (2,5-dimethyl-2,5-bis (tert-butylperoxy) hexane).

Ubushyuhe bwo gukiza nigihe cyagenwe ukurikije ingano yibicuruzwa nuburyo bwo gukiza bwakozwe nabakiriya.

Gupakira ibicuruzwa


Iki gicuruzwa ni ibicuruzwa bidateza akaga, gupakira amakarito, igikapu cya pulasitike imbere, ibiro icumi kumufuka, imifuka ibiri kumasanduku.

Igihe cyo kubika


Kubera ko iki gicuruzwa gifite imitekerereze ikonje, mugihe cyo gutwara no gukoresha umufuka ugomba kwirinda kumeneka.

Ubike ahantu hakonje, humye ubuzima bwamezi 12.

Mbere: 
Ibikurikira: 

LINKS

IBICURUZWA BYACU

AMAKURU

Ongeraho: No.33, Umuhanda 159, Umuhanda wa Taiye, Akarere ka Fengxian, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Uburenganzira     2023 Shanghai Herchy Rubber Co., Ltd. Ikarita |   Politiki Yibanga | Inkunga Na Kurongora.