FV9600 Fluorosilicone

O lenei oloa e lelei le mu, faʻafeiloaʻi le UL94/FV 0 le maualuga o le mumu. E sili atu le malosi o le suauʻu, faʻamaʻi soli, maualuga ma maualalo le vevela avanoa
  • FV9600

  • Herchy

Avanoa:
Aofaʻi:

Fa'ailoga fa'apitoa

Aitema

Fa'asinomaga

Vasega

FV9660

FV9670

Fa'aaliga

Metotia Su'ega

Lanu pa'epa'e

Gravity Fa'apitoa/g/cm3

ASTM D792

1.46

1.48

Ma'a'a / matafagaA

ASTM D2240

60

70

Malosi Tetele/MPa

ASTM D412

6.8

6.5

Fa'aumi ile malologa /%

ASTM D412

310

290

Malosi Loimata/KN/m

ASTM D624-B

17

17

* Tete'e vevela
200 ℃ × 72h

Suiga ma'a'a / matafaga A

+5

+5

Suiga le malosi o le tese,%

3.8

3.5

Suiga le malosi o le tese,%

161

154

IRM903
Suiga Volume/%
150℃/72h

ASTM D471

5.5

5.2

Suau'u C
Fuainumera fua o suiga/%
23℃/72h

ASTM D471

20

20

Tulaga e taofia ai le afi

GBT10707-2008

FV 0

FV 0

Tulaga Fa'amalolo

Fa'aopoopo 0.7 vaega o le bis(2+5), tasi vaega vulcanisation 170℃×15min, lua vaega vulcanisation: 200℃×4h.


Fautuaga mo le fa'agaioiina


Fa'aaoga le 0.6 i le 1 vaega o le bis-dipenta vulcanising agent(2,5-dimethyl-2,5-bis(tert-butylperoxy)hexane).

O le vevela vevela ma le taimi e filifili e tusa ai ma le tele o le oloa ma le auala e faʻamalo ai e le tagata faʻatau.

Fa'apipi'i o Oloa


O lenei oloa o 'oloa e le mata'utia, fa'apipi'i pusa, taga palasitika afifi totonu, sefulu kilokalama i le ato, lua taga i le pusa.

Taimi e teu ai


Talu ai o lenei oloa o loʻo i ai mea malulu, i le taimi o felauaiga ma le faʻaaogaina o le ato e tatau ona aloese mai le gau.

Teu i se nofoaga malulu ma matutu e teu ai le 12 masina.

Muamua: 
Sosoo ai: 

SO'OGA VAIVAI

OA TATOU Oloa

FA'AALIGA FESOASOANI

Faʻaopoopo: Nu.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Telefoni / WhatsApp / Skype: +86 15221953351
Puletaofia     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap |   Faiga Fa'alilolilo | Lagolago e Leadong.