Tel: +8615221953351   E-mail: info@herchyrubber.com
PRODUCTS
You are here: Home » Products » Synthesis Rubber » FVMQ Fluorosilicone » FV9600 Fluorosilicone

loading

Share to:
facebook sharing button
twitter sharing button
line sharing button
wechat sharing button
linkedin sharing button
pinterest sharing button
whatsapp sharing button
sharethis sharing button

FV9600 Fluorosilicone

This product has good flame retardancy, meet UL94/FV 0 flame retardant level. Excellent oil resistance, solvent resistance, high and low temperature resistance
  • FV9600

  • Herchy

Availability:
Quantity:

Technical indicators

Items

Index

Grade

FV9660

FV9670

Appearance

Test Methods

White

Specific Gravity/g/cm3

ASTM D792

1.46

1.48

Hardness/shoreA

ASTM D2240

60

70

Tensile Strength/MPa

ASTM D412

6.8

6.5

Elongation At Break /%

ASTM D412

310

290

Tear Strength/KN/m

ASTM D624-B

17

17

*Heat Resistance
200℃×72h

Hardness change /shore A

+5

+5

Tensile strength change, %

3.8

3.5

Tensile strength change, %

161

154

IRM903
Volume Change/%
150℃/72h

ASTM D471

5.5

5.2

Fuel C
Volumetric rate of change/%
23℃/72h

ASTM D471

20

20

Flame-retardant Level

GBT10707-2008

FV  0

FV  0

Curing Condition

Add 0.7 parts of bis(2+5), one stage vulcanisation 170℃×15min, two stage vulcanisation: 200℃×4h.


Processing recommendations


Use 0.6 to 1 part bis-dipenta vulcanising agent(2,5-dimethyl-2,5-bis(tert-butylperoxy)hexane).

The curing temperature and the time are decided according to the size of the product and the method of curing carried out by the customer.

Product Packaging


This product is Non-dangerous goods, carton packaging, plastic bag inner packaging, ten kilograms per bag, two bags per box.

Storage period


Since this product has cold flow properties, during the transportation and in use the bag should be avoided to be broken.

Store in cool, dry place shelf life 12 months.

Previous: 
Next: 

QUICK LINKS

OUR PRODUCTS

CONTACT INFORMATION

Add: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +8615221953351
Copyright  2023 Shanghai Herchy Rubber Co., Ltd. Sitemap |  Privacy Policy | Support By Leadong.