FV9600 Fluorosilicone

He pai te mura o tenei hua, ka tutuki ki te UL94/FV 0 te taumata mura. He tino pai te atete hinu, te whakarewa whakarewa, te teitei me te iti o te pāmahana parenga
  • FV9600

  • Herchy

Wātea:
Rahi:

Tohu Hangarau

Nga taonga

Taurangi

Kōeke

FV9660

FV9670

Te ahua

Nga Tikanga Whakamatau

Taumaha Tauwhāiti/g/cm3

ASTM D792

1.46

1.48

Te pakeke/tatahiA

ASTM D2240

60

70

Te Kaha Toka/MPa

ASTM D412

6.8

6.5

Whakaroa I te Whati /%

ASTM D412

310

290

Te Kaha Roimata/KN/m

ASTM D624-B

17

17

*Atete Wea
200℃×72h

Huri pakeke / takutai A

+5

+5

Hurihia te kaha kaha, %

3.8

3.5

Hurihia te kaha kaha, %

161

154

IRM903
Huringa Rōrahi/%
150℃/72h

ASTM D471

5.5

5.2

Wāhi C
Te tere o te hurihanga/%
23℃/72h

ASTM D471

20

20

Taumata mura

GBT10707-2008

FV 0

FV 0

Tikanga Whakaora

Taapirihia kia 0.7 nga wahanga o te bis(2+5), kotahi te wahanga whakangao 170℃×15min, e rua nga wahanga whakangao: 200℃×4h.


Tukatuka tohutohu


Whakamahia te 0.6 ki te 1 wahanga bis-dipenta vulcanising agent(2,5-dimethyl-2,5-bis(tert-butylperoxy)hexane).

Ko te pāmahana whakaora me te wa ka whakatauhia i runga i te rahi o te hua me te tikanga o te rongoa i mahia e te kaihoko.

Whakapaipai Hua


Ko tenei hua he taonga Kore morearea, he kete kaata, he peeke kirihou te takai o roto, tekau kirokaramu mo ia peeke, e rua peeke mo ia pouaka.

Te wa rokiroki


I te mea he ahua makariri tenei hua, i te wa e kawe ana me te whakamahi me karohia te peeke kia pakaru.

Rokiroki ki roto i te waahi makariri, maroke te ora mo te 12 marama.

Tōmua: 
Panuku: 

NGA LINKO Tere

O TATOU HUA

HE KORERO WHAKAPAKI

Tāpirihia: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Waea / WhatsApp / Skype: +86 15221953351
Ī-mēra:  info@herchyrubber.com
Mana pupuri     2023 Shanghai Herchy Rubber Co., Ltd. Mahere pae |   Kaupapahere Tūmataiti | Tautoko Na Leadong.