Aikace-aikace: dace da samar da zafi stamping cots, zafi stamping farantin, zafi canja wuri nadi, copier nadi, da dai sauransu.
Siffofin maɓalli: kyakkyawan juriya ga babba da ƙananan zafin jiki (60 'C -350 'C), ƙarfin juriya mai kyau da juriya mai kyau, ƙananan nakasar saiti, mai wuyar lalacewa da karaya, tsawon rayuwar sabis.
Gwaji: 1% na wakili mai warkarwa (manna 50% na DBPMH a cikin danko silicone),175'C x 5min x 15MPa.
| Siffofin samfur | ||||||
| Samfura | GA-5750 | GA-5770 | GA-5780 | GA-5741 | GA-5761 | |
| Bayyanar | Hoary | Fait rawaya | ||||
| Hardness (ShoreA) | 55 | 70 | 80 | 43 | 60 | |
| Ƙarfin ɗaure (MPa) | 5.5 | 6 | 7 | 6 | 8 | |
| Tsawaita(%) | 230 | 150 | 100 | 400 | 350 | |
| Ƙarfin hawaye (kN/m) | 10 | 9 | 9 | 15 | 25 | |
| 175'C x22h Matsi(%) | 8 | 10 | 10 | 10 | 10 | |