GA-8961 ƒe agbalẽa
Herchy ƒe ame
| Nusiwo Li: | |
|---|---|
| Agbɔsɔsɔ: | |
Dodokpɔ: 0.5% le DBPMH me, 175° xminx 15MPa.
| Nusiwo wowɔ ƒe nɔnɔmewo | ||||||
| Nu si wowɔ | GA-8961 ƒe agbalẽa |
GA-8961W ƒe agbalẽ | ||||
| Dzedzeme | Yibᴐ | Ɣi |
||||
| Sesẽme (ƑutaA) . |
40 |
52 |
58 |
70 |
80 |
53 |
| Eƒe kpekpeme(g/cm3) . | 1.38 |
1.38 |
1.40 |
1.50 |
1.52 |
1.44 |
| Ŋusẽ si wotsɔna ƒoa nu (MPa) . |
4.5 |
5.5 |
5.5 |
5.0 |
4.5 |
7.0 |
| Elongation(%) ƒe didime . | 380 |
400 |
350 |
300 |
170 |
400 |
| Aɖatsi ƒe ŋusẽ (kN/m) . | 20 |
17.0 |
15 |
14 |
12 |
15 |
| Dzobibi ƒe dzeside/ 1 mm |
UL94V-0 ƒe ƒuƒoƒo |
|||||
| UL ƒe faɛl ƒe xexlẽdzesi | E484677 ye nye esia |
-- . |
||||