GA-8961 Karet silikon tahan api (sertifikat UL) (HCR)

Aplikasi: kabeh jinis produk flame-retardant.
Fitur utama: halogen-freeflame retardant, flame retardant banget, tahan panas sing apik, lulus otentikasi RoHS lan REACH.
  • GA-8961

  • Herchy

kasedhiyan:
Jumlah:

Tes: 0,5% saka DBPMH, 175° xminx 15MPa.

Parameter produk
produk GA-8961
GA-8961W
Penampilan ireng Putih
Kekerasan (ShoreA)
40
52
58
70
80
53
Kapadhetan (g/cm3) 1.38
1.38
1.40
1.50
1.52
1.44
Kekuatan tarik (MPa)

4.5
5.5
5.5
5.0
4.5
7.0
Elongasi (%) 380
400
350
300
170
400
Kekuwatan sobek (kN/m) 20
17.0
15
14
12
15
Kelas tahan api / 1 mm
UL94V-0
Nomer berkas UL E484677
--









Sadurunge: 
Sabanjure: 

LINKS CEPAT

PRODUK KAMI

INFORMASI KONTAK

Tambah: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Telpon / WhatsApp / Skype: +86 15221953351
Hak Cipta     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap |   Kebijakan Privasi | Dhukungan dening Leadong.