GA-8961 Omupiira gwa silikoni oguziyiza ennimi z’omuliro (UL certificated) (HCR)

Okukozesa: Ebintu eby’engeri zonna ebiziyiza ennimi z’omuliro.
Ebikulu: Halogen-freeflame retardant, okulwala ennimi z’omuliro ennungi ennyo, okuziyiza okw’amaanyi, okuyisa okukakasa kwa RoHs n’okutuuka.
  • GA-8961 .

  • Herchy .

Obudde:
Omuwendo:

Okugezesa: 0.5% ku DBPMH, 175° Xminx 15MPa.

Ebipimo by'ebintu .
Ekyamaguzi GA-8961 .
GA-8961W .
Endabika Obuddugavu Kyeeru
Obukakanyavu (Shorea) .
40
52
58
70
80
53
Densite(g/cm3) . 1.38
1.38
1.40
1.50
1.52
1.44
Amaanyi g’okusika (MPA) .

4.5
5.5
5.5
5.0
4.5
7.0
okuwanvuwa(%) . 380
400
350
300
170
400
Amaanyi g’okukutuka (kn/m) . 20
17.0
15
14
12
15
Ekipimo ky’okuziyiza ennimi z’omuliro/ 1 mm .
UL94V-0.
Ennamba ya fayiro ya UL . E484677 .
-- .









Jjuuzi: 
Ekiddako: 

Enkolagana ez'amangu .

Ebintu byaffe .

Ebikwata ku bantu

Add: No.33, Lane 159, Oluguudo lwa Taiye, Disitulikiti y’e Fengx, Shanghai
Essimu / WhatsApp / Skype: +86 15221953351
Eddembe ly’okuwandiika     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap . |   Enkola y'Ebyama | Obuwagizi bwa . Leadong ..