GA-8961
Herchy
| Ketersediaan: | |
|---|---|
| Kuantiti: | |
Ujian: 0.5% daripada DBPMH, 175° xminx 15MPa.
| Parameter produk | ||||||
| produk | GA-8961 |
GA-8961W | ||||
| Penampilan | Hitam | putih |
||||
| Kekerasan (ShoreA) |
40 |
52 |
58 |
70 |
80 |
53 |
| Ketumpatan(g/cm3) | 1.38 |
1.38 |
1.40 |
1.50 |
1.52 |
1.44 |
| Kekuatan tegangan (MPa) |
4.5 |
5.5 |
5.5 |
5.0 |
4.5 |
7.0 |
| Pemanjangan(%) | 380 |
400 |
350 |
300 |
170 |
400 |
| Kekuatan koyakan (kN/m) | 20 |
17.0 |
15 |
14 |
12 |
15 |
| Gred kalis api/ 1 mm |
UL94V-0 |
|||||
| Nombor fail UL | E484677 |
-- |
||||