GA-8961 Pa'u silikoni e taofia le mu (UL certificated) (HCR)

Fa'aoga: ituaiga uma o mea e fa'afefeteina afi.
Autu autu: halogen-freeflame retardant, sili ona lelei le mu, faʻafefete lelei, pasi le faʻamaoniga o le RoHS ma le REACH.
  • GA-8961

  • Herchy

Avanoa:
Aofaiga:

Su'ega: 0.5% o DBPMH, 175 ° xminx 15MPa.

Fa'atauga o oloa
Oloa GA-8961
GA-8961W
Fa'aaliga Lanu uliuli Lanu pa'epa'e
Malosi (ShoreA)
40
52
58
70
80
53
Malosi (g/cm3) 1.38
1.38
1.40
1.50
1.52
1.44
Malosi fa'amalosi (MPa)

4.5
5.5
5.5
5.0
4.5
7.0
Fa'atele(%) 380
400
350
300
170
400
Malosi o loimata (kN/m) 20
17.0
15
14
12
15
Vasega fa'asa'o mumu/ 1 mm
UL94V-0
UL faila numera E484677
--









Muamua: 
Sosoo ai: 

SO'OGA VAIVAI

OA TATOU Oloa

FA'AMATALAGA FESOASOANI

Faʻaopoopo: Nu.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Telefoni / WhatsApp / Skype: +86 15221953351
Puletaofia     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap |   Faiga Fa'alilolilo | Lagolago e Leadong.