GA-8961
Herchy
| Ri fhaotainn: | |
|---|---|
| Meud: | |
Deuchainn: 0.5% de DBPMH, 175 ° xminx 15MPa.
| Paramadairean toraidh | ||||||
| Bathar | GA-8961 |
GA-8961W | ||||
| Coltas | Dubh | Geal |
||||
| cruas (CladachA) |
40 |
52 |
58 |
70 |
80 |
53 |
| Dlùths (g/cm3) | 1.38 |
1.38 |
1.40 |
1.50 |
1.52 |
1.44 |
| Neart tensile (MPa) |
4.5 |
5.5 |
5.5 |
5.0 |
4.5 |
7.0 |
| Leudachadh (%) | 380 |
400 |
350 |
300 |
170 |
400 |
| Neart deòir (kN/m) | 20 |
17.0 |
15 |
14 |
12 |
15 |
| Ìre dìon-lasair / 1 mm |
UL94V-0 |
|||||
| Àireamh faidhle UL | E484677 |
-- |
||||