GA-8961
Herchy
| Kasadiaan: | |
|---|---|
| Kuantitas: | |
Uji: 0,5% tina DBPMH, 175 ° xminx 15MPa.
| Parameter produk | ||||||
| produk | GA-8961 |
GA-8961W | ||||
| Penampilan | Hideung | Bodas |
||||
| Teu karasa (ShoreA) |
40 |
52 |
58 |
70 |
80 |
53 |
| Kapadetan (g/cm3) | 1.38 |
1.38 |
1.40 |
1.50 |
1.52 |
1.44 |
| Kakuatan tegangan (MPa) |
4.5 |
5.5 |
5.5 |
5.0 |
4.5 |
7.0 |
| Elongation(%) | 380 |
400 |
350 |
300 |
170 |
400 |
| Kakuatan cimata (kN/m) | 20 |
17.0 |
15 |
14 |
12 |
15 |
| Kelas tahan seuneu / 1 mm |
UL94V-0 |
|||||
| Nomer file UL | E484677 |
-- |
||||