GA-8961 Flame-Shostant Rolicone (Asambodo UL) (HCR)

Ngwa: Valdị ngwaahịa a na-ere ọkụ.
Atụmatụ igodo: Halogen-Freeflame Lardflant, ezigbo ezumike, nguzogide, na-egbochi nkwenye nke Rohs wee ruo.
  • Ga-8961

  • Herchy

Nnweta:
Ọnụ ọgụgụ:

Nwalee: 0,5% nke DBPMh, 175 Celsius Xminx 15MPa.

Poramita ngwaahịa
Ihe emeputara ohuru Ga-8961
Ga-8961W
Mputa Oji Ucha
Ihe siri ike (Shorea)
40
52
58
70
80
53
Nnọọ (G / CM3) 1.38
1.38
1.40
1.50
1.52
1.44
Ike TESILE (MPA)

4.5
5.5
5.5
5.0
4.5
7.0
Elongation (%) 380
400
350
300
170
400
Ike (kn / m) 20
17.0
15
14
12
15
Glame laradent / 1 mm
UL94V-0
Nọmba Nel Faịlụ E484677
- -









Nke gara aga: 
Osote: 

Njikọ ngwa ngwa

Ngwaahịa anyị

OZI MKPỌTỤRỤ

Tinye: Mba.33, Lane 159, Taiye Road, District FENDXIE, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Copyright     2023 Shanghai rọtchy rọba Co., LTD. Pe |   Amụma Nzuzo | Nkwado site na Ndukwa.