GA-8961
Herchy
| Wātea: | |
|---|---|
| Rahi: | |
Whakamātautau: 0.5% o DBPMH, 175° xminx 15MPa.
| Tawhā hua | ||||||
| Hua | GA-8961 |
GA-8961W | ||||
| Te ahua | Pango | Mā |
||||
| Maama (ShoreA) |
40 |
52 |
58 |
70 |
80 |
53 |
| Kiato(g/cm3) | 1.38 |
1.38 |
1.40 |
1.50 |
1.52 |
1.44 |
| Te kaha o te kaha (MPa) |
4.5 |
5.5 |
5.5 |
5.0 |
4.5 |
7.0 |
| Whakaroa(%) | 380 |
400 |
350 |
300 |
170 |
400 |
| Te kaha roimata (kN/m) | 20 |
17.0 |
15 |
14 |
12 |
15 |
| Koeke mura ahi/ 1 mm |
UL94V-0 |
|||||
| UL tau kōnae | E484677 |
-- |
||||