GA-8961 ya go swana le yona
Herchy ya go swana le
| Go hwetšagala: | |
|---|---|
| Palo: . | |
Teko: 0.5% ya DBPMH, 175 ° xminx 15MPa.
| Ditekanyetšo tša setšweletšwa | ||||||
| Setšweletšwa | GA-8961 ya go swana le yona |
GA - 8961W | ||||
| Ponagalo | Ntsho | Tšhweu |
||||
| Thata (LebopoA) . |
40 |
52 |
58 |
70 |
80 |
53 |
| Kitlano (g / cm3) . | 1.38 |
1.38 |
1.40 |
1.50 |
1.52 |
1.44 |
| Matla a go goga (MPa) . |
4.5 |
5.5 |
5.5 |
5.0 |
4.5 |
7.0 |
| Go telefatšwa(%) . | 380 |
400 |
350 |
300 |
170 |
400 |
| Matla a go gagola (kN/m) . | 20 |
17.0 |
15 |
14 |
12 |
15 |
| Mophato wa go thibela kgabo/ 1 mm |
UL94V-0 ya go tšhungwa |
|||||
| Nomoro ya faele ya UL | E484677 |
-- . |
||||