GA-91X3B Silicone rɔba a ɛyɛ den a ɛko tia (tuntum) (HCR) .

Dwumadi: ɛfata ma wɔyɛ antistatic silicone rollers,antistatic gasket,mobile fixtures, mfiridwuma ahorow ahorow ne nea ɛkeka ho.
Nneɛma atitiriw: antistatic agyapade betumi akora so daa, hightemperature baking resistant, twam nokwaredi a RoHS ne REACH.
  • GA-91X3B na ɛwɔ hɔ

  • Herchy a ɔyɛ ɔbarima

Nea Ɛwɔ Hɔ:
Dodow:

Sɔhwɛ: 1% a ɛyɛ aduru a wɔde sa yare (50% a wɔde DBPMH a wɔde ahyɛ silicone gum mu), 175° x5minx15MPa


Nneɛma a wɔyɛ no parameters
Adwadeɛ GA-9153B na ɛwɔ hɔ GA-9163B na ɛwɔ hɔ GA-9173B na ɛwɔ hɔ GA-9183B na ɛwɔ hɔ
Mmaeɛ Tuntum
Nneɛma a ɛyɛ den (ShoreA) .
50
60
70
80
Nsuo a ɛyɛ den(g/cm3) . 1.16
1.18
1.21
1.22
Ahoɔden a wɔde twe ade (MPa) .

9.0
8.0
7.0
7.0
Ntrɛwmu(%) . 500
400
300
150
Ahoɔden a ɛtetew mu (kN/m) . 20
20
16
16
Nneɛma a ɛwɔ soro a ɛko tia(Ω) . 105--106









Dada: 
Deɛ ɛdi hɔ: 

NKYERƐKYERƐMU A ƐYƐ NTƐM

NKYERƐKYERƐMU A ƐFA NKYERƐKYERƐMU HO

Fa ka ho: No.33, Ɔkwan 159, Taiye Kwan, Fengxian Mantam, Shanghai
Tɛlɛ / WhatsApp / Skype: +86 15221953351 wobɛtumi akyerɛw wo din
Nneɛma a wɔde yɛ adwuma     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap a Wɔde Di Dwuma |   Kokoam Nsɛm Ho Nhyehyɛe | Mmoa a Wɔde Ma Leadong na ɛwɔ hɔ.