GA-91X0
Herchy
| Saadavus: | |
|---|---|
| Kogus: | |
Test: 1% kõvendit (50% DBPMH pasta silikoonkummis), 175° x 5 min x 15 MPa
| Toote parameetrid | |||||
| Toode | GA-9130 |
GA-9140 | GA-9150 | GA-9160 | GA-9170 |
| Välimus | Läbipaistev | ||||
| Williamplastilisus |
150 |
190 |
250 |
280 |
300 |
| Kõvadus (ShoreA) |
30 |
40 |
50 |
60 |
70 |
| Tihedus (g/cm3) | 1.11 |
1.14 |
1.17 |
1.20 |
1.21 |
| Tõmbetugevus (MPa) |
8.0 |
9.5 |
10.0 |
9.0 |
8.5 |
| pikenemine (%) | 900 |
700 |
600 |
500 |
400 |
| Rebimistugevus (kN/m) | 17 |
20 |
25 |
25 |
25 |
| Pinnatakistus (Ω) | 1011 |
||||