GA-91X0
Herchy
| samuwa: | |
|---|---|
| Yawan: | |
Gwaji: 1% na wakili mai warkarwa (50% manna DBPMH a cikin danko silicone), 175° x5minx15MPa
| Siffofin samfur | |||||
| Samfura | GA-9130 |
GA-9140 | GA-9150 | GA-9160 | GA-9170 |
| Bayyanar | Translucent | ||||
| Williamplasticity |
150 |
190 |
250 |
280 |
300 |
| Hardness ( ShoreA) |
30 |
40 |
50 |
60 |
70 |
| Girma (g/cm3) | 1.11 |
1.14 |
1.17 |
1.20 |
1.21 |
| Ƙarfin ɗaure (MPa) |
8.0 |
9.5 |
10.0 |
9.0 |
8.5 |
| Tsawaita(%) | 900 |
700 |
600 |
500 |
400 |
| Ƙarfin hawaye (kN/m) | 17 |
20 |
25 |
25 |
25 |
| Juriyar saman (Ω) | 1011 |
||||