GA-91X0 Antistatic silicone rubber (fumed silica) (HCR)

Applicatio: applicabilis ad electronicos antistaticos producendos, sicut in vagina, cylindro.
Clavis lineamenta: magna vis, insulsa, optima antistatica proprietas, theauthenticatio RoHS et SPATIUM transi.
  • GA-91X0

  • Herchy

Availability:
Quantity:

Test: 1% curationis agentis (50% crustulum DBPMH in gummi siliconis), 175° x5minx15MPa

Product parametri
Productum GA-9130
GA-9140 GA-9150 GA-9160 GA-9170
Aspectus Translucens
Williamplasticity
150
190
250
280
300
Duritia (ShoreA)
30
40
50
60
70
Densitas (g/cm3) 1.11
1.14
1.17
1.20
1.21
Roboris distrahentes (MPa)

8.0
9.5
10.0
9.0
8.5
Prolongatio(%) 900
700
600
500
400
Robur scindere (kN/m) 17
20
25
25
25
Superficies resistentia (Ω) 1011









Previous: 
Next: 

ORIGINAL LINKS

Our Products

Contact Information

Add: No.33, Lane CLIX, Taiye via, Fengxian District, Shanghai
Tel / whatsapp / Skype: +86 15221953351
Copyright     2023 Shanghai Herchy Flexilis Co., Ltd. Sitemap |   Privacy Policy | Support By Leadong.