GA-91X0 rapa silicone antistatic (hika wera) (HCR)

Taupānga: tono ki te whakaputa i nga hua hiko antistatic, penei i te kopaki, roera.
Ko nga ahuatanga matua: te kaha nui, te reka, te taonga antistatic pai, te whakamana i te RoHS me te REACH.
  • GA-91X0

  • Herchy

Wātea:
Rahi:

Whakamatau: 1% o te kaihoko whakaora (50% te whakapiri o te DBPMH i roto i te kapia silicone), 175° x5minx15MPa

Tawhā hua
Hua GA-9130
GA-9140 GA-9150 GA-9160 GA-9170
Te ahua Puatarangi
Williamplasticity
150
190
250
280
300
Maama (ShoreA)
30
40
50
60
70
Kiato(g/cm3) 1.11
1.14
1.17
1.20
1.21
Te kaha o te kaha (MPa)

8.0
9.5
10.0
9.0
8.5
Whakaroa(%) 900
700
600
500
400
Te kaha roimata (kN/m) 17
20
25
25
25
Ātete mata(Ω) 1011









Tōmua: 
Panuku: 

NGA LINKO Tere

O TATOU HUA

HE KORERO WHAKAPAKI

Tāpirihia: No.33, Lane 159, Taiye Road, Takiwa Fengxian, Shanghai
Waea / WhatsApp / Skype: +86 15221953351
Ī-mēra:  info@herchyrubber.com
Mana pupuri     2023 Shanghai Herchy Rubber Co., Ltd. Mahere pae |   Kaupapahere Tūmataiti | Tautoko Na Leadong.