GA-27X0 LSR ya Switirhisiwa swa Vutshunguri (LSR) .

Ku tirhisiwa: tinxaka to hambana ta saccule, catheter na switirhisiwa swin’wana swa vutshunguri
Swihlawulekisi swa nkoka: ku vonakala lokunene na matimba ya le henhla, ku hundza theauthentication ya 1S010993 biological compatibity test.
  • GA-2720

  • Herchy

Ku kumeka:
Nhlayo: .

Xikambelo: Nhlayo ya A/B ya 1 :1, 130°C x 5min x 15MPa


Tipharamitha ta swikumiwa
Ximakiwa GA-2720 GA-2730 GA-2740 GA-2750 GA-2760 GA-2770
Xivumbeko Erivaleni

Ku tsindziyela(Pa.s) .
2000 3000 3000 3500
4000 5000
Ku nonoka (ShoreA) . 20 30 40 50
60
70
Ku tsindziyela(g/cm3) . 1.10 1.10 1.11 1.12 1.1.3
1.14
Ku tiya ka ku tsana (MPa) . 7.0
8.0
9.5
10.0
10.0
9.5
Ku leha(%) . 880 800 700 550 500
350
Matimba ya ku handzuka (kN/m) . 16 30 35
40 35
30
Ku hunguteka ka milayeni(%) . 2.1 2.1 2.1 2.0 2.0
2.0








Endzhaku: 
Landzelaka: 

XITLHOKOVETSELO XA XITLHANYI

SWILO SWA HINA

VUXOKOXOKO BYA VUXOKOXOKO

Engetelani: No.33, Lane 159, Gondzo ra Taiye, Xifundzha xa Fengxian, Shanghai
Riqingho / WhatsApp / Skype: +86 15221953351
Vukorhokeri bya Vutshila     2023 Shanghai Herchy Rubber Co., Ltd. Mepe wa sayiti |   Pholisi ya Vuhlayiseki | Nseketelo Hi Leadong.