GA-99XX Wajiga Uumiga Silica Xoojinta Isku-xidhka Hoose ee Silicone Rubber (HCR)
Codsiga: ku habboon soo saarista giraanta xidhitaanka, sariiraha, qaybaha baabuurta iyo alaabada kale.
Tilmaamaha muhiimka ah: adkeysi sare, go'an cadaadis hooseeya, HSE aan dhadhan lahayn, gudbin xaqiijinta RoHS, REACH iyo FDA.
Tijaabada: 1% wakiilka daweynta (50% koollada DBPMH ee xanjada silikoonka), 175心5minx 15MPa.
| Xuduudaha alaabta | |||||||
| Alaabta | GA-9930 | GA-9935H | GA-9935 | GA-9940 | GA-9950 | GA-9960 | GA-9970T |
| Muuqashada | Translucent | Caanaha Caanaha | Translucent | ||||
| Williamplasticity | 120 | 140 | 130 | 140 | 160 | 200 | 250 |
| Adag ( ShoreA) | 30 | 33 | 36 | 40 | 50 | 60 | 70 |
| Cufnaanta (g/cm3) | 1.1 | 1.1 | 1.1 | 1.11 | 1.12 | 1.15 | 1.17 |
| Xoog xajin (MPa) | 7 | 9.5 | 9.5 | 8 | 9 | 9 | 9.5 |
| Dheeraynta(%) | 700 | 800 | 700 | 600 | 400 | 300 | 250 |
| Xoogga jeexjeexa (kN/m) | 15 | 15 | 15 | 15 | 20 | 20 | 20 |
| 175 'C x22h cadaadis(%) | 15 | 20 | 15 | 15 | 15 | 15 | 15 |