GA-91X1 Caag Silikoon Antistatic ah (Silica Roobka leh) (HCR)

Shanghai Herchy Rubber Co., Ltd., waxaanu ku siinaynaa caag heer sare ah oo joogto ah (HCR) oo ku habboon warshadaha dalbanaya waxqabad sare iyo isku hallayn. Alaabtayada GA-91X1 waxay isku daraysaa sifooyin antistatic heer sare ah, oo bixiya ilaalin gaar ah oo ka dhan ah dareeraha korantada. Marka lagu daro silica degdega ah, caaggu wuxuu ilaaliyaa sifooyin farsamo oo aad u fiican, oo ay ku jiraan xoogga adag ee adag iyo adkeysiga. Haddii aad u baahan tahay agabka codsiyada elektarooniga ah, shaabadihii, ama qaybaha kale ee saxda ah, waxaanu hubinaynaa in badeecad kastaa ay la kulanto heerarka warshadaha oo ku habboon shuruudahaaga gaarka ah.
  • GA-91X1

  • Herchy

Helitaanka:
Tirada:

Horudhaca GA-91X1 Kastasta Silicone Antistatic (HCR)


GA-91X1 Antistatic Silicone Rubber (HCR) oo leh silica soo degtay waa shay horumarsan oo loogu talagalay iska caabin koronto oo heer sare ah iyo adkaysi farsamo. Caag-joogta sare leh (HCR) waxaa loogu talagalay codsiyada warshadaha ee u baahan iska caabin hoose oo dusha sare ah iyo kala daadsanaan taagan.


Taxanahan caagga ah ee silikoonku wuxuu bixiyaa waxqabad heersare ah oo ka jira jawiga xakamaynta dareeraha korantada (ESD) ay lagama maarmaan tahay. Waxay ku habboon tahay codsiyada elektarooniga, wax soo saarka, iyo warshadaha kale ee u baahan agab xasaasi ah.


Taxanaha GA-91X1 waxaa ku jira noocyo badan oo leh heerar adag oo kala duwan, taasoo ka dhigaysa mid aad loo habeyn karo si loo daboolo baahiyahaaga waxqabad ee gaarka ah. Haddii aad u baahan tahay adkeysi sare ama dabacsanaan la xoojiyey, alaabtan waxaa loo qaabayn karaa si ay ugu habboonaato shuruudaha codsigaaga.


Waxyaabaha gaarka ah ee caagga ah waxaa ka mid ah xoog farsamo oo xoog leh, dabacsanaan aad u fiican, iyo iska caabin sare oo xirashada. Muuqaalka translucent wuxuu bixiyaa muuqaal wanaagsan, taas oo ah faa'iidada muhiimka ah ee jawiga warshadaha kala duwan.


Tijaabada: 1% ee wakiilka daawaynta (50% koollada DBPMH ee xanjada silikoonka), 175° x5minx15MPa


Tilmaamaha Alaabta


Xuduudaha alaabta
Alaabta GA-9131
GA-9141 GA-9151 GA-9161 GA-9171
Muuqashada Translucent
Williamplasticity
120
140
200
240
270
Adag ( ShoreA)
30
40
50
60
70
Cufnaanta (g/cm3) 1.11
1.14
1.17
1.18
1.19
Xoog xajin (MPa)

7.0
8.0
8.5
10.0
9.5
Dheeraynta(%) 700
600
700
600
500
Xoogga jeexjeexa (kN/m) 15
18
35
35
35
Iska caabinta dusha sare (Ω)
1011


Waxaan bixinaa habayn buuxda oo loogu talagalay GA-91X1 Antistatic Silicone Rubber, oo ay ku jiraan hagaajinta engegnaanta, cufnaanta, iyo guryaha kale ee jirka. Haddii aad raadinayso shuruudo waxqabad oo gaar ah ama astaamo naqshadeed oo gaar ah, kooxdayada khabiiradu waxay diyaar u yihiin inay kaa caawiyaan xalalka loo habeeyey mashruucaaga.


GA-91X1 Antistatic Silicone Rubber


GA-91X1 Antistatic Silicone Rubber Features


The GA-91X1 Antistatic Silicone Rubber, oo leh silica soo degtay, waxay bixisaa ilaalinta dareeraha korantada ee aad u wanaagsan (ESD) ee codsiyada elegtarooniga ah ee xasaasiga ah.


Astaamaha Muhiimka ah

  • Waxqabadka heersare ee antistatic: Waxay bixisaa iska caabin hoose oo dusha sare ah oo loogu talagalay kontoroolka ESD ee la isku halayn karo ee alaabta elektiroonigga ah.

  • Aan ur lahayn oo badbaado leh: Waxay ku habboon tahay warshadaha u baahan aan sun ahayn, caag silikoon ammaan ah oo loogu talagalay jawi xasaasi ah.

  • RoHS iyo REACH u hoggaansan: Waxay buuxisaa heerarka deegaanka ee badbaadada iyo xeerarka kiimikada ee suuqa caalamiga ah.

  • Adkeysiga iyo dabacsanaanta: Xoogga sare ee xajinta iyo dhererka ayaa hubiya alaabada caaga ah ee silikoon ee dheer, xitaa xaaladaha adag.


Codsiyada

  • Qaybaha Elektaroonigga ah: Waxay ku fiican yihiin gacmo-gashi caag ah, rollers, iyo alaabada kale ee caagga silikoon ee loo isticmaalo aaladaha elegtarooniga ah ee xasaasiga ah.

  • Qalabka ka-hortagga-static: Si ballaaran loogu isticmaalo warshadaha u baahan xalal caag antistatic ah oo loogu talagalay baakadaha, kaydinta, iyo maaraynta.


Su'aalaha Iyo Jawaabaha Inta Badan La Isweydiiyo


Q1: Waa maxay isticmaalka aasaasiga ah ee GA-91X1 Antistatic Silicone Rubber?
A1: Waxay ku habboon tahay codsiyada elektarooniga ah ee xasaasiga ah ESD, sida gacmo-gashi ilaalin ah iyo rullalusha.


Q2: GA-91X1 caag silikoon ah ma u hoggaansamo heerarka badbaadada caalamiga ah?
A2: Haa, waxay la kulmeysaa u hoggaansanaanta RoHS iyo REACH ee amniga iyo xeerarka deegaanka.


Q3: Ma u habeyn karaa GA-91X1 caag silikoon ah shuruudo gaar ah?
A3: Haa, waxaanu bixinaa xalal ku habboon si loo daboolo cabbirkaaga gaarka ah, adkaantaada, iyo baahiyaha waxqabadka.


Q4: Sidee GA-91X1 u bixisaa guryaha antistatic?
A4: Halabuurka caagga ah ee leh silica degdega ah waxay hubisaa iska caabbinta dusha hoose ee ilaalinta ESD la isku halayn karo.


Q5: GA-91X1 ma ku haboon yahay in lagu isticmaalo deegaan adag?
A5: Haa, adkaysigeeda iyo dabacsanaanteeda ayaa ka dhigaysa mid u adkaysata xidhashada oo waxtar leh marka la eego shuruudaha baahida.


Q6: Ma dalban karaa GA-91X1 caag silikoon heerar adag oo kala duwan?
A6: Haa, waxaan bixinaa xulashooyin adag oo badan si aan ugu dhigno shuruudaha codsi ee kala duwan.


Q7: Waa maxay warshadaha ka faa'iideysan kara GA-91X1 caag silikoon antistatic?
A7: Waxaa si weyn loogu isticmaalaa qalabka elektiroonigga ah, baabuurta, iyo warshadaha wax soo saarka u baahan in la xakameeyo taagan.


Q8: Sidee GA-91X1 gacan uga geysan kartaa tayada alaabta iyo badbaadada?
J8: Waxay kaa caawinaysaa dhimista dhaawaca la xidhiidha fadhiidnimada, hubinta maaraynta badbaadada leh iyo baakaynta qalabka elegtarooniga ah ee xasaasiga ah.

Kii hore: 
Xiga: 

XIDHIIDHYADA DEGDEGGA AH

Alaabooyinkayaga

MACLUUMAADKA XIRIIRKA

Kudar: No.33, Lane 159, Wadada Taiye, Degmada Fengxian, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Xuquuqda daabacaadda     2023 Shanghai Herchy Rubber Co., Ltd. Khariidadda goobta |   Siyaasadda Qarsoonnimada | Taageerada By Leadong.