GA-97XX
Herchy
| Helitaanka: | |
|---|---|
| Tirada: | |
GA-97XX Caag Silikoon u adkaysta Saliida (HCR)
Codsiga: ku habboon wax soo saarka saliidda u adkaysta.
Astaamaha muhiimka ah: xoog sare, dulqaad wanaagsan oo leh ASTM 1 # iyo IRM903 Saliid, dhaaf xaqiijinta RoHS iyo REACH.
Tijaabada: 1% ee wakiilka daawaynta (50% koollada DBPMH ee xanjada silikoonka), 175°Cx5min x15MPa.
| Xuduudaha alaabta | |||||
| Alaabta | GA-9740 | GA-9750 | GA-9760 | GA-9770 | |
| Muuqashada | Cawlan | ||||
| Williamplasticity | 140 | 180 | 200 | 260 | |
| Adag ( ShoreA) | 40 | 50 | 60 | 70 | |
| Cufnaanta (g/cm3) | 1.23 | 1.25 | 1.28 | 1.32 | |
| Xoog xajin (MPa) | 3.5 | 4.5 | 5 | 5.5 | |
| Dheeraynta(%) | 700 | 600 | 400 | 250 | |
| Xoogga jeexjeexa (kN/m) | 15 | 15 | 15 | 15 | |
| 175 'C x22h cadaadis(%) | 20 | 20 | 20 | 20 | |
| Duqowga hawada 225°C x70H | Adaggu wuu is beddelaa | 1 | 2 | 2 | 2 |
| Heerka isbeddelka xoogga kacsanaanta | -25% | -25% | -25% | -25% | |
| Heerka isbeddelka dhererka | -30% | -30% | -30% | -30% | |
| IRM903 Saliid 150°C x70H | Adaggu wuu is beddelaa | -18 | -18 | -17 | -16 |
| Heerka isbeddelka xoogga kacsanaanta | -35% | -35% | -35% | -35% | |
| Heerka isbeddelka dhererka | -20% | -20% | -20% | -20% | |
| Bedelka mugga | 36% | 36% | 35% | 35% | |