High Strength Oil Resistance Seal Chloroprene Rubber-CR
Appearance: beige lumps, non-contaminating
Regulator type: sulfur and xanthate mixture regulator
Crystallization speed: medium
Menni viscosity ML1+4(100℃): 46-55
Effective period: below 20℃, 1 year; 20-30℃, half a year;
Packing: lined with polyethylene film, jacketed with kraft paper polypropylene compilation bag, net content of 25kg per