Agbara Oil Resistance Seal Chloroprene Rubber-CR
Irisi: alagara lumps, ti kii-contaminating
Olutọsọna iru: efin ati xanthate adalu eleto
Crystallization iyara: alabọde
Menni viscosity ML1 + 4 (100 ℃): 46-55
munadoko akoko: labẹ 20 ℃, 1 odun; 20-30 ℃, idaji odun kan;
Iṣakojọpọ: ti o ni ila pẹlu fiimu polyethylene, jaketi pẹlu apo akopọ polypropylene iwe kraft, akoonu apapọ ti 25kg fun