Oil chakna sang tak nei Seal Chloroprene Rubber-CR
A lan dan: beige lumps, bawlhhlawh lo
Regulator chi: sulfur leh xanthate mixture regulator
Crystallization speed: medium
Menni viscosity ML1+4(100°C): 46-55
A hman hun chhung: 20°C hnuai lam, kum 1 20-30°C, kum chanve chhung;
Packing: polyethylene film hmanga lined, kraft paper polypropylene compilation bag hmanga jacket, net content 25kg per