High Strength Oil Resistance Seal Chloroprene Rubber-CR
Hitsura: beige lumps, non-contaminating
Regulator type: sulfur and xanthate mixture regulator
Bilis ng crystallization: medium
Menni lagkit ML1+4(100℃): 46-55
Effective period: below 20℃, 1 taon; 20-30 ℃, kalahating taon;
Pag-iimpake: nilagyan ng polyethylene film, naka-jacket ng kraft paper polypropylene compilation bag, net content na 25kg bawat