Fanga caman tulu bɛ se ka kɛ ka chloroprene lastikuw-cr .
Yecogo: kurukuru beige, nɔgɔ tɛ min na
Regulateur suguya: kisɛ ni xantate ɲagaminen ɲɛnabɔbaga
Kristali teliya: cɛmancɛ
Menni sɔgɔsɔgɔninjɛ ML1+4(100°C): 46-55
A daminɛ waati: 20°C duguma, san 1 20-30°C, san tilancɛ;
A foroko : a datugulen don ni poliyetilɛni filimu ye, a jatigila ni kraft papier poliporopilini dalajɛ bɔrɔ ye, a hakɛ jɛlen ye kilo 25 ye kelen na