Njira Zabwino Zopangira Misozi Lamba la Chloroprene Rubber-CR
Maonekedwe: zotupa za beige kapena zofiirira, zosaipitsa
Mtundu wa Regulator: sulfure ndi xanthate mix regulator
Kuthamanga kwa Crystallization: medium
Menni viscosity ML1 + 4 (100 ℃): 30-45
Nthawi yogwira ntchito: pansi pa 20 ℃, 1 chaka; 20-30 ℃, theka la chaka;
Kulongedza: alimbane ndi filimu polyethylene, jekete ndi kraft pepala polypropylene compilation thumba, ukonde zili 25kg / thumba