Appearance and condition: white (transparent or translucent) blocky Third monomer type and content: ENB, 6.5% Ethylene content: 68% Mooney viscosity: ML(1+4)125°C 135 Size: 25kg/block MOQ: 25kg Packing: boxed
Appearance and condition: white (transparent or translucent) blocky Third monomer type and content: ENB, 4.7% Ethylene content: 70% Oil content:75% Mooney viscosity: ML(1+4)125°C 62 Size: 25kg/block MOQ: 25kg Packing: boxed
Appearance and condition: white (transparent or translucent) blocky Third monomer type and content: ENB, 4.1% Ethylene content: 58% Mooney viscosity: ML(1+4)125°C 84 Size: 25kg/block MOQ: 25kg Packing: boxed
Appearance: White to yellowish powder Znic oxide Content:88-93% Heavy metal as Pb2+ (%): 0.001 Max. Copper as Cu2+ (%): 0.0005 Max. Manganese as Mn2+ (%): 0.001 Max. Density(g/mm3):4.6 Specific surface area(m2/g):40
Appearance: White to yellowish powder Znic oxide Content:min 90% Heavy metal as Pb2+ (%): 0.001 Max. Copper as Cu2+ (%): 0.0005 Max. Manganese as Mn2+ (%): 0.001 Max. Density(g/mm3):3.6 Specific surface area(m2/g):40
Appearance: White to yellowish powder Znic oxide Content:min 40% Heavy metal as Pb2+ (%): 0.002 Max. Copper as Cu2+ (%): 0.001 Max. Manganese as Mn2+ (%): 0.001 Max.