Fa'amaufa'ailoga Suau'u Fa'asa'o Mamalu Maualuga Chloroprene Rubber-CR
Fa'aaliga: lumps beige, le fa'aleagaina
Ituaiga Pulea: sulfur ma le xanthate fa'afefiloiga fa'amalo
Saosaoa fa'ama'i: vaeluaga
Menni viscosity ML1+4(100℃): 46-55
Vaitaimi aoga: i lalo ole 20℃, 1 tausaga; 20-30 ℃, afa tausaga;
afifiina: laina i le polyethylene ata tifaga, peleue i le pepa kraft polypropylene compilation ato, upega i totonu o le 25kg i le