GA-2002 na mokanda
HERCHY .
| Disponibilité: | |
|---|---|
| Quantité: | |
Momekano: Rapport A/B ya 1 :1, 130°C x 5min x 15MPa
| Ba paramètres ya produit | |||||||
| Eloko | GA-2002 na mokanda | GA-2003 na mokanda | GA-2004 na mokanda | GA-2005 na mokanda | GA-2006 | GA-2007 | |
| Komonana | Ezomonana na kati | ||||||
| Bokasi ya makasi (ShoreA) . | 23 | 30 | 40 | 50 |
62 |
68 |
|
| Densité(g/cm3) Ezali na ba . | 1.10 | 1.12 | 1.12 | 1.13 | 1.14 |
1.14 |
|
| Bokasi ya kokangama (MPa) . | 6.0 |
8.0 |
9.0 |
9.0 |
10.0 |
9.5 |
|
| Elongation(%) ya . | 750 | 650 | 600 | 500 | 450 |
400 |
|
| Bokasi ya kopasola (kN/m) . | 10 | 15 | 20 |
25 | 30 |
35 |
|
| Contenu ya VOC(%) . | 0.35 | 0.35 | 0.3 | 0.3 | 0.3 | 0.3 | |