GA-200X Okenn Kawotchou silikon likid apre geri (LSR)

Aplikasyon: apwopriye pou pwodwi tibebe, tankou pwent tete ti bebe, boutèy ti bebe, elatriye.
Karakteristik kle: ba matyè temèt, segondè transparans, ekselan pwopriyete mekanik, pase otantifikasyon RoHS, REACH, FDA, ak LFGB
  • GA-2002

  • Herchy

Disponibilite:
Kantite:

Tès: A/B rapò 1:1, 130°C x 5min x 15MPa


Paramèt pwodwi
Pwodwi GA-2002 GA-2003 GA-2004 GA-2005 GA-2006 GA-2007
Aparans Transparan

Dite (ShoreA) 23 30 40 50
62
68
Dansite (g/cm3) 1.10 1.12 1.12 1.13 1.14
1.14
Fòs rupture (MPa) 6.0
8.0
9.0
9.0
10.0
9.5
elongasyon (%) 750 650 600 500 450
400
Fòs chire (kN/m) 10 15 20
25 30
35
Kontni VOC (%) 0.35 0.35 0.3 0.3 0.3 0.3







Previous: 
Pwochen: 

Lyen RAPID

PWODWI NOU YO

ENFÒMASYON KONTAK

Add: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Dwa     2023 Shanghai Herchy Rubber co, Ltd. Sitemap |   Règleman sou enfòmasyon prive | Sipòte By Leadong.