GA-26X0 Trè transparan ak gwo fòs LSR (LSR)

Aplikasyon: apwopriye pou pwodwi founiti pou kwizin wo-fen, founiti pou naje, founiti pou ti bebe, elatriye.
Karakteristik kle: segondè fòs, segondè transparans, klas manje, pase otantifikasyon RoHS, REACH, FDA ak LFGB.
  • GA-2610

  • Herchy

Disponibilite:
Kantite:

Tès: A/B rapò 1:1, 130°C x 5min x 15MPa



Paramèt pwodwi


Pwodwi GA-2610 GA-2620 GA-2630 GA-2640 GA-2650 GA-2660 GA-2670 GA-2680
Aparans Transparan



Viskozite (Pa.s)
1500 2000 2500 3000 3500 4000
4000
5500
Dite (ShoreA) 10 20 30 40 50
60
70
80
Dansite (g/cm3) 1.08 1.10 1.10 1.11 1.12
1.13
1.14
1.15
Fòs rupture (MPa) 4.5
6.5
7.5
9.5
10.0
10.0
9.5
9.0
elongasyon (%) 900 880 800 700 550
450
350
350
Fòs chire (kN/m) 8 12 15 25 35
35
30
30
lineyè kontraksyon (%) 2.3 2.1 2.1 2.1 2.0
2.0
2.0
2.0
Transmisyon (%) 90
90 90 90 90 90 90 90




Previous: 
Pwochen: 

Lyen RAPID

PWODWI NOU YO

ENFÒMASYON KONTAK

Add: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Dwa     2023 Shanghai Herchy Rubber co, Ltd. Sitemap |   Règleman sou enfòmasyon prive | Sipòte By Leadong.