GA-2610
Herchy
| Ri fhaotainn: | |
|---|---|
| Meud: | |
Deuchainn: Co-mheas A/B de 1:1, 130°C x 5min x 15MPa
| Paramadairean toraidh | |||||||||
| Bathar | GA-2610 | GA-2620 | GA-2630 | GA-2640 | GA-2650 | GA-2660 | GA-2670 | GA-2680 | |
| Coltas | follaiseach | ||||||||
| Slaodachd (Pas) |
1500 | 2000 | 2500 | 3000 | 3500 | 4000 |
4000 |
5500 |
|
| cruas (CladachA) | 10 | 20 | 30 | 40 | 50 |
60 |
70 |
80 |
|
| Dlùths (g/cm3) | 1.08 | 1.10 | 1.10 | 1.11 | 1.12 |
1.13 |
1.14 |
1.15 |
|
| Neart tensile (MPa) | 4.5 |
6.5 |
7.5 |
9.5 |
10.0 |
10.0 |
9.5 |
9.0 |
|
| Leudachadh (%) | 900 | 880 | 800 | 700 | 550 |
450 |
350 |
350 |
|
| Neart deòir (kN/m) | 8 | 12 | 15 | 25 | 35 |
35 |
30 |
30 |
|
| Lùghdachadh loidhneach (%) | 2.3 | 2.1 | 2.1 | 2.1 | 2.0 |
2.0 |
2.0 |
2.0 |
|
| Tar-chuir (%) | 90 |
90 | 90 | 90 | 90 | 90 | 90 | 90 | |