Ulapha: Ikhaya » Imikhiqizo » Irabha Yokuhlanganisa » I-Silicone ye-VMQ GA -26X0 Highly-transparent And High Strength LSR (LSR)

iyalayisha

Yabelana ku-:
inkinobho yokwabelana ye-facebook
inkinobho yokwabelana ye-twitter
inkinobho yokwabelana ngomugqa
inkinobho yokwabelana ye-wechat
inkinobho yokwabelana ye-linkedin
inkinobho yokwabelana ye-pinterest
inkinobho yokwabelana ye-whatsapp
yabelana ngale nkinobho yokwabela

I-GA-26X0 Highly-transparent And High Strength LSR (LSR)

Isicelo: ilungele ukukhiqiza izinto zasekhishini ezisezingeni eliphezulu, izinto zokubhukuda, izinsiza zezingane, njll.
Izici ezibalulekile: amandla aphezulu, ukukhanya okuphezulu, ibanga lokudla, kuphumelele ukuqinisekiswa kwe-RoHS, REACH, FDA kanye ne-LFGB.
  • GA-2610

  • I-Herchy

Ukutholakala:
Ubuningi:

Isivivinyo: A/B isilinganiso 1 :1, 130°C x 5min x 15MPa



Imingcele yomkhiqizo


Umkhiqizo GA-2610 GA-2620 GA-2630 GA-2640 GA-2650 GA-2660 GA-2670 GA-2680
Ukubukeka Okusobala



I-Viscosity(Pa.s)
1500 2000 2500 3000 3500 4000
4000
5500
Ukuqina (ShoreA) 10 20 30 40 50
60
70
80
Ukuminyana(g/cm3) 1.08 1.10 1.10 1.11 1.12
1.13
1.14
1.15
Amandla e-Tensile (MPa) 4.5
6.5
7.5
9.5
10.0
10.0
9.5
9.0
Ubude(%) 900 880 800 700 550
450
350
350
Amandla wezinyembezi (kN/m) 8 12 15 25 35
35
30
30
Ukuncipha komugqa(%) 2.3 2.1 2.1 2.1 2.0
2.0
2.0
2.0
I-Transmittance(%) 90
90 90 90 90 90 90 90




Okwedlule: 
Okulandelayo: 

IZIXHUMANISI EZISHESHAYO

IMIKHIQIZO YETHU

ULWAZI LOKUXHUMANA

Engeza: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Ucingo / WhatsApp / Skype: +86 15221953351
I-imeyili:  info@herchyrubber.com
Copyright     2023 Shanghai Herchy Rubber Co., Ltd. Imephu yesayithi |   Inqubomgomo Yobumfihlo | Sekela Ngu I-Leadong.