Ucingo: +86 15221953351 I-imeyili: info@herchyrubber.com
Please Choose Your Language
IMIKHIQIZO
Ulapha: Ikhaya » Imikhiqizo » Irabha Yokuhlanganisa » I-Silicone ye-VMQ GA -27X0 LSR for Medical Qroducts (LSR)

iyalayisha

Yabelana ku-:
inkinobho yokwabelana ye-facebook
inkinobho yokwabelana ye-twitter
inkinobho yokwabelana ngomugqa
inkinobho yokwabelana ye-wechat
inkinobho yokwabelana ye-linkedin
inkinobho yokwabelana ye-pinterest
inkinobho yokwabelana ye-whatsapp
yabelana ngale nkinobho yokwabela

I-GA-27X0 LSR for Medical Qroducts (LSR)

Isicelo: izinhlobo ezahlukene ze-saccule, i-catheter neminye imikhiqizo yezokwelapha
Izici ezibalulekile: ukukhanya okuhle kakhulu namandla aphezulu, kuphumelele ukuqinisekiswa kwe-1S010993 ukuhlolwa kokuhambisana kwezinto eziphilayo.
  • GA-2720

  • I-Herchy

Ukutholakala:
Ubuningi:

Isivivinyo: A/B isilinganiso 1 :1, 130°C x 5min x 15MPa


Imingcele yomkhiqizo
Umkhiqizo GA-2720 GA-2730 GA-2740 GA-2750 GA-2760 GA-2770
Ukubukeka Okusobala

I-Viscosity(Pa.s)
2000 3000 3000 3500
4000 5000
Ukuqina (ShoreA) 20 30 40 50
60
70
Ukuminyana(g/cm3) 1.10 1.10 1.11 1.12 1.1.3
1.14
Amandla e-Tensile (MPa) 7.0
8.0
9.5
10.0
10.0
9.5
Ubude(%) 880 800 700 550 500
350
Amandla wezinyembezi (kN/m) 16 30 35
40 35
30
Ukuncipha komugqa(%) 2.1 2.1 2.1 2.0 2.0
2.0








Okwedlule: 
Olandelayo: 

IZIXHUMANISI EZISHESHAYO

IMIKHIQIZO YETHU

ULWAZI LOKUXHUMANA

Engeza: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Ucingo / WhatsApp / Skype: +86 15221953351
I-imeyili:  info@herchyrubber.com
Copyright     2023 Shanghai Herchy Rubber Co., Ltd. Imephu yesayithi |   Inqubomgomo Yobumfihlo | Sekela Ngu I-Leadong.