I-GA-93X0 yokuzithela i-silicone ruble (i-silica eqondile) (HCR)

Isicelo: Kufanelekile ukukhiqizwa kwamapulaki wokubopha kanye neminye imikhiqizo.
Isici esiyisihluthulelo: Impahla enhle yokopha uwoyela, okuqukethwe kawoyela kungaphezu kuka-7%, kudlulise ukuthundla kwama-rohs nokufinyelela.
  • Ga-93x0

  • Umkhelo

Ukutholakala:
Inani:

Ukuhlola: 1% we-ejenti yokulapha (50% unamathisela we-DBPMH in 小 conegum), 175 ° C x 5min x 15mpa.


Amapharamitha Womkhiqizo
Umphumela Ga-9330 Ga-9340 I-GA-9350 Ga-9360 Ga-9370
Ukubonakala I-MilkyWhite
I-Williamplasticity 140 170 200 220 240
Ubulukhuni (Shorea) 30 40 50 60 70
Ubuningi (G / CM3) 1.12 1.14 1.17 1.2 1.21
Amandla we-Tensile (MPA) 9 10 10 8.5 8.5
I-Elongation (%) 850 800 700 500 350
Amandla ezinyathelani (KN / M) 20 25 30 25 25


Okwedlule: 
Olandelayo: 

Izixhumanisi ezisheshayo

Imikhiqizo yethu

ULWAZI LOKUXHUMANA

Faka: Cha.33, Umzila 159, Taiye Road, Fenghian District, Shanghai
I-TEL / WhatsApp / Skype: +86 15221953351
I-imeyili:  info@herchyrubber.com
I-copyright     2023 Shanghai Herchy Rubber Co, Ltd. Indawo lapho ittamap |   Inqubomgomo Yobumfihlo | Ukusekelwa ngu Govong.