Ucingo: +86 15221953351 I-imeyili: info@herchyrubber.com
Please Choose Your Language
IMIKHIQIZO
Ulapha: Ikhaya » Imikhiqizo » Irabha Yokuhlanganisa » Irabha Ye-Silicone Engazweli Ngamafutha I-Silicone ye-VMQ I -GA-97XX (HCR)

iyalayisha

Yabelana ku-:
inkinobho yokwabelana ye-facebook
inkinobho yokwabelana ye-twitter
inkinobho yokwabelana ngomugqa
inkinobho yokwabelana ye-wechat
inkinobho yokwabelana ye-linkedin
inkinobho yokwabelana ye-pinterest
inkinobho yokwabelana ye-whatsapp
yabelana ngale nkinobho yokwabela

I-GA-97XX Irabha Ye-Silicone Engazweli Kawoyela (HCR)

I-GA-97XX Irabha Ye-Silicone Engazweli Kawoyela (HCR)
Isicelo: ilungele ukukhiqizwa kwemikhiqizo ephikisana namafutha.
Izici ezibalulekile: amandla aphezulu, ukubekezelelana okuhle nge-ASTM 1# kanye ne-IRM903 Amafutha, kudlule ukuqinisekiswa kwe-RoHS kanye ne-REACH.
 
  • GA-97XX

  • I-Herchy

Ukutholakala:
Ubuningi:

I-GA-97XX Irabha Ye-Silicone Engazweli Kawoyela (HCR)


Isicelo: ilungele ukukhiqizwa kwemikhiqizo ephikisana namafutha.
Izici ezibalulekile: amandla aphezulu, ukubekezelelana okuhle nge-ASTM 1# kanye ne-IRM903 Amafutha, kudlule ukuqinisekiswa kwe-RoHS kanye ne-REACH.
Ukuhlolwa: 1% we-ejenti yokwelapha (50% unamathise we-DBPMH ku-silicone gum), 175°Cx5min x15MPa.



Imingcele yomkhiqizo
Umkhiqizo GA-9740 GA-9750 GA-9760 GA-9770
Ukubukeka Okumpunga
Williamplasticity 140 180 200 260
Ukuqina (ShoreA) 40 50 60 70
Ukuminyana(g/cm3) 1.23 1.25 1.28 1.32
Amandla e-Tensile (MPa) 3.5 4.5 5 5.5
Ubude(%) 700 600 400 250
Amandla wezinyembezi (kN/m) 15 15 15 15
175'C x22h Ukucindezela(%) 20 20 20 20
Ukuguga komoya okungu-225°C x70H Ukuqina kokuqina 1 2 2 2
Izinga lokushintsha amandla e-tension -25% -25% -25% -25%
Izinga lokushintsha kobude -30% -30% -30% -30%
I-IRM903 uwoyela 150°C x70H Ubunzima bushintsha -18 -18 -17 -16
Izinga lokushintsha amandla e-tension -35% -35% -35% -35%
Izinga lokushintsha kobude -20% -20% -20% -20%
Ukushintsha kwevolumu 36% 36% 35% 35%


Okwedlule: 
Olandelayo: 

IZIXHUMANISI EZISHESHAYO

IMIKHIQIZO YETHU

ULWAZI LOKUXHUMANA

Engeza: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Ucingo / WhatsApp / Skype: +86 15221953351
I-imeyili:  info@herchyrubber.com
Copyright     2023 Shanghai Herchy Rubber Co., Ltd. Imephu yesayithi |   Inqubomgomo Yobumfihlo | Sekela Ngu I-Leadong.