Ga-90 ×x Platnomu caliconzed silikoni roba fun igba idinku (3R)

Ohun elo: dara fun iṣelọpọ okun, rinhoho roba, idana, ati bẹbẹ lọ 
Awọn ẹya ara ẹrọ pataki: Funmoration ati airotẹlẹ ti ohun-ini ati majele ti ko ni ijẹrisi, Dide, FDA ati LFGB.
  • Ga-9041

  • Egbo

Wiwa:
Iwọn:

Idanwo: Aṣẹ Platenum Creplanizing, 130 ° C X 5min x 15mpa.

Ọja Awọn ọja
Ọja Ga-9041
Ga-9051 Ga-9061 Ga-9071 Ga-9081
Ifarahan Atinuri
Williaty
190
210
240
270
290
Lile (sheaa)
40
50
60
70
80
Iwuwo (g / cm3) 1.13
1.16
1.18
1.19
1.21
Agbara Tensele (MPA)

9.0
10.0
10.0
9.5
9.0
Piglesation (%) 900
700
600
500
400
Agbara yiya (Kni / M) 30
35
35
35
35










Ti tẹlẹ: 
Itele: 

Awọn ọna asopọ iyara

Awọn ọja wa

IBI IWIFUNNI

Ṣafikun: Bẹẹkọ
Tes / Whatsapp / Skype: +86 15221953351
Aṣẹ-ara     2023 Shanghai Herchy Herchy Co., LtD. Oju-oju opo |   Eto Afihan | Atilẹyin nipasẹ Agbero.