GA-93X0
Herchy
| Boteng: | |
|---|---|
| Bongata: | |
Teko: 1% ea moriana (50% peista ea DBPMH ins小conegum), 175°C x 5min x 15MPa.
| Lihlahisoa tsa lihlahisoa | |||||
| Sehlahisoa | GA-9330 | GA-9340 | GA-9350 | GA-9360 | GA-9370 |
| Ponahalo | MilkyWhite | ||||
| Williamplasticity | 140 | 170 | 200 | 220 | 240 |
| Ho thatafala (LebopoA) | 30 | 40 | 50 | 60 | 70 |
| Boima ba 'mele(g/cm3) | 1.12 | 1.14 | 1.17 | 1.2 | 1.21 |
| Tensile Matla (MPa) | 9 | 10 | 10 | 8.5 | 8.5 |
| Elongation(%) | 850 | 800 | 700 | 500 | 350 |
| Matla a ho lla (kN/m) | 20 | 25 | 30 | 25 | 25 |