ꯖꯤ.ꯑꯦ.-꯲꯰꯰꯲ꯗꯥ ꯊꯣꯀꯈꯤ꯫
ꯍꯔꯆꯤ꯫
| ꯐꯪꯂꯤꯕꯥ: | |
|---|---|
| ꯃꯁꯤꯡ: | |
ꯇꯦꯁ꯭ꯠ: 1 :1, 130°C x 5min x 15MPaꯒꯤ A/B ꯔꯦꯁꯤꯑꯣ꯫
| ꯄ꯭ꯔꯗꯛꯇ ꯄꯦꯔꯥꯃꯤꯇꯔꯁꯤꯡ꯫ | |||||||
| ꯄꯣꯠꯊꯣꯛ | ꯖꯤ.ꯑꯦ.-꯲꯰꯰꯲ꯗꯥ ꯊꯣꯀꯈꯤ꯫ | ꯖꯤ.ꯑꯦ.-꯲꯰꯰꯳ꯗꯥ ꯖꯤ.ꯑꯦ | ꯖꯤ.ꯑꯦ.-꯲꯰꯰꯴ꯗꯥ ꯖꯤ.ꯑꯦ | ꯖꯤ.ꯑꯦ.-꯲꯰꯰꯵ꯗꯥ ꯊꯣꯀꯈꯤ꯫ | ꯖꯤ.ꯑꯦ.-꯲꯰꯰꯶ꯇꯥ ꯊꯣꯀꯈꯤ꯫ | ꯖꯤ.ꯑꯦ.-꯲꯰꯰꯷ꯇꯥ ꯊꯣꯀꯈꯤ꯫ | |
| ꯃꯄꯥꯟꯊꯣꯡꯗ ꯎꯕ | ꯅꯨꯡ ꯄꯥꯟ ꯐꯥꯎꯅ ꯎꯕ | ||||||
| ꯍꯥꯔꯗꯅꯦꯁ (ꯁꯣꯔꯑꯦ) ꯑꯃꯁꯨꯡ ꯑꯦꯟ. | 23 | 30 | 40 | 50 |
62 |
68 |
|
| ꯗꯦꯟꯁꯤꯇꯤ(ꯖꯤ/ꯁꯦ.ꯃꯤ.꯳) ꯑꯁꯤꯅꯤ꯫ | 1.10 | 1.12 | 1.12 | 1.13 | 1.14 |
1.14 |
|
| ꯇꯦꯟꯁꯥꯏꯜ ꯁ꯭ꯠꯔꯦꯡꯊ (ꯑꯦꯝ.ꯄꯤ.ꯑꯦ.) ꯑꯃꯁꯨꯡ ꯑꯦꯝ.ꯄꯤ.ꯑꯦ. | 6.0 |
8.0 |
9.0 |
9.0 |
10.0 |
9.5 |
|
| ꯏꯂꯣꯡꯒꯦꯁꯟ(%) ꯴. | 750 | 650 | 600 | 500 | 450 |
400 |
|
| ꯇꯤꯌꯥꯔ ꯁ꯭ꯠꯔꯦꯡꯊ (kN/m) ꯑꯁꯤꯅꯤ꯫ | 10 | 15 | 20 |
25 | 30 |
35 |
|
| ꯚꯤ.ꯑꯣ.ꯁꯤ.ꯒꯤ ꯆꯥꯡ(%) . | 0.35 | 0.35 | 0.3 | 0.3 | 0.3 | 0.3 | |