GA-91X3B reberi yo mu rwego rwo hejuru anticatic silicone rubber (umukara) (HCR)

Gushyira mu bikorwa: bikwiranye no gukora ibizunguzungu bya antisatike ya silicone, gasike ya antistatike, ibikoresho bigendanwa, inganda zitandukanye n'ibindi.
Ibyingenzi byingenzi: umutungo wa antistatike urashobora kugumana burundu, kwihanganira guteka cyane, gutambutsa ibyemezo bya RoHS na REACH.
  • GA-91X3B

  • Herchy

Kuboneka:
Umubare:

Kwipimisha: 1% yumuti ukiza (50% paste ya DBPMH mumase ya silicone), 175 ° x5minx15MPa


Ibipimo byibicuruzwa
Ibicuruzwa GA-9153B GA-9163B GA-9173B GA-9183B
Kugaragara Umukara
Gukomera (ShoreA)
50
60
70
80
Ubucucike (g / cm3) 1.16
1.18
1.21
1.22
Imbaraga zingana (MPa)

9.0
8.0
7.0
7.0
Kurambura (%) 500
400
300
150
Amarira amarira (kN / m) 20
20
16
16
Kurwanya Ubuso (Ω) 105--106









Mbere: 
Ibikurikira: 

LINKS

IBICURUZWA BYACU

AMAKURU

Ongeraho: No.33, Umuhanda 159, Umuhanda wa Taiye, Akarere ka Fengxian, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Uburenganzira     2023 Shanghai Herchy Rubber Co., Ltd. Ikarita |   Politiki Yibanga | Inkunga Na Kurongora.