Ọdịdị na ọnọdụ: ọcha (transperent ma ọ bụ translucent) blocky
Ụdị monomer nke atọ na ọdịnaya: ENB, 6.5%
Ethylene ọdịnaya: 68%
Mooney viscosity: ML (1 + 4) 125 ° C 135
Size: 25kg / igbochi
MOQ: 25kg
Mbukota: boxed
Ọdịdị na ọnọdụ: ọcha (transparent ma ọ bụ translucent) blocky
Ụdị monomer nke atọ na ọdịnaya: ENB, 4.1%
Ethylene ọdịnaya: 58%
Mooney viscosity: ML (1 + 4) 125 ° C 84
Size: 25kg / igbochi
MOQ: 25kg
Mbukota: boxed
Ọdịdị: White na-acha odo odo ntụ ntụ
Znic oxide ọdịnaya: 88-93%
metal dị arọ dị ka Pb2 + (%): 0.001 Max.
Ọla kọpa dị ka Cu2+ (%): 0.0005 Max.
Manganese dị ka Mn2+ (%): 0.001 Max.
Njupụta (g/mm3): 4.6
Specific elu mpaghara (m2/g): 40
Ọdịdị: Ọcha na-acha odo odo ntụ ntụ
Znic oxide ọdịnaya: min 90%
metal dị arọ dị ka Pb2 + (%): 0.001 Max.
Ọla kọpa dị ka Cu2+ (%): 0.0005 Max.
Manganese dị ka Mn2+ (%): 0.001 Max.
Njupụta (g/mm3): 3.6
Specific elu mpaghara (m2/g): 40
Ọdịdị: Ọcha na-acha odo odo ntụ ntụ
Znic oxide ọdịnaya: min 40%
metal dị arọ dị ka Pb2 + (%): 0.002 Max.
Ọla kọpa dị ka Cu2+ (%): 0.001 Max.
Manganese dị ka Mn2+ (%): 0.001 Max.