A lan dan leh a dinhmun: var (transparent emaw translucent emaw) blocky
Third monomer chi leh a awm zat: ENB, 6.5%
Ethylene awm zat: 68%
Mooney viscosity: ML(1+4)125°C 135
Size: 25kg/block
MOQ: 25kg
Packing: boxed
A lan dan leh a dinhmun: White (Transparent or Translucent) Blocky
Third monomer chi leh a thupui: ENB, 4.7%
Ethylene awm zat: 70%
Oil awm zat:75%
Mooney viscosity: ML(1+4)125°C 62
Size: 25KG/Block
Moq: 25KG
Packing: Boxed
A lan dan leh a dinhmun: var (transparent emaw translucent emaw) blocky
Third monomer chi leh a awm zat: ENB, 4.1%
Ethylene awm zat: 58%
Mooney viscosity: ML(1+4)125°C 84
Size: 25kg/block
MOQ: 25kg
Packing: boxed
A lan dan: Powder dum atanga sen hring
Znic oxide A awm zat:88-93%
Heavy metal as Pb2+ (%): 0.001 Max.
Copper chu Cu2+ (%) angin: 0.0005 Max.
Manganese chu Mn2+ (%) angin: 0.001 Max.
Density(g/mm3):4.6
A zau zawng bik(m2/g):40
A lan dan: Powder dum atanga sen hring
Znic oxide A awm zat:min 90%
Heavy metal as Pb2+ (%): 0.001 Max.
Copper chu Cu2+ (%) angin: 0.0005 Max.
Manganese chu Mn2+ (%) angin: 0.001 Max.
Density(g/mm3):3.6
A zau zawng bik(m2/g):40
A lan dan: Powder dum atanga sen hring
Znic oxide A awm zat:min 40%
Heavy metal as Pb2+ (%): 0.002 Max.
Copper chu Cu2+ (%) angin: 0.001 Max.
Manganese chu Mn2+ (%) angin: 0.001 Max.