Irisi: Funfun si yellowish powder
Znic oxide Akoonu: min 90%
Eru irin bi Pb2 + (%): 0.001 Max.
Ejò bi Cu2+ (%): 0.0005 Max.
Manganese bi Mn2+ (%): 0.001 Max.
Ìwúwo (g/mm3):3.6
Agbegbe dada kan pato (m2/g): 40
Irisi: Funfun si yellowish lulú
Znic oxide Akoonu: min 40%
Eru irin bi Pb2 + (%): 0.002 Max.
Ejò bi Cu2+ (%): 0.001 Max.
Manganese bi Mn2+ (%): 0.001 Max.