Hitsura at kondisyon: puti (transparent o translucent) blocky
pangatlong uri ng monomer at nilalaman: ENB, 6.5%
nilalaman ng etilena: 68%
viscosity ng mooney: ml (1+4) 125 ° C 135
Sukat: 25kg/block
moq: 25kg
packing: boxed
Hitsura at kondisyon: puti (transparent o translucent) blocky
pangatlong uri ng monomer at nilalaman: ENB, 4.7%
Ethylene Nilalaman: 70%
Nilalaman ng langis : 75%
Mooney Viscosity: ML (1+4) 125 ° C 62
Sukat: 25kg/Block
MOQ: 25kg
Packing: Boxed
Hitsura at kondisyon: puti (transparent o translucent) blocky
pangatlong uri ng monomer at nilalaman: ENB, 4.1%
Ethylene Nilalaman: 58%
Mooney Viscosity: ML (1+4) 125 ° C 84
Sukat: 25kg/Block
MOQ: 25kg
Packing: Boxed
Hitsura: Puti hanggang Dilaw na Powder
Znic Oxide Nilalaman: 88-93%
mabibigat na metal bilang PB2+ (%): 0.001 max.
Copper bilang Cu2+ (%): 0.0005 max.
Manganese bilang Mn2+ (%): 0.001 max.
Density (g/mm3) : 4.6
Tukoy na lugar ng ibabaw (M2/g) : 40
Hitsura: Puti hanggang Dilaw na Powder
Znic Oxide Nilalaman: Min 90%
mabibigat na metal bilang PB2+ (%): 0.001 max.
Copper bilang Cu2+ (%): 0.0005 max.
Manganese bilang Mn2+ (%): 0.001 max.
Density (g/mm3) : 3.6
Tukoy na lugar ng ibabaw (M2/g) : 40
Hitsura: Puti hanggang Dilaw na Powder
Znic Oxide Nilalaman: Min 40%
mabibigat na metal bilang PB2+ (%): 0.002 max.
Copper bilang Cu2+ (%): 0.001 max.
Manganese bilang Mn2+ (%): 0.001 max.