Te ahua me te ahua: ma (maamaa ranei) poraka
Tuatoru momo monomer me te ihirangi: ENB, 6.5%
Ethylene ihirangi: 68%
Mooney viscosity: ML(1+4)125°C 135
Rahi: 25kg/poraka
MOQ: 25kg
Te takai: pouaka
Te ahua me te ahua: ma (maamaa, maamaa ranei) poraka
Tuatoru momo monomer me te ihirangi: ENB, 4.7%
Ethylene ihirangi: 70%
Te hinu hinu: 75%
Mooney viscosity: ML(1+4)125°C 62
Rahi: 25kg/poraka
MOQ: 25kg
Te takai: pouaka
Te ahua me te ahua: ma (maamaa ranei) poraka
Tuatoru momo monomer me te ihirangi: ENB, 4.1%
Ethylene ihirangi: 58%
Mooney viscosity: ML(1+4)125°C 84
Rahi: 25kg/poraka
MOQ: 25kg
Te takai: pouaka
Te ahua: Ma ki te kowhai te paura
Znic oxide Ihirangi: 88-93%
Te whakarewa taimaha hei Pb2+ (%): 0.001 Max.
Te parahi hei Cu2+ (%): 0.0005 Max.
Konupora hei Mn2+ (%): 0.001 Max.
Kiato(g/mm3):4.6
Horahanga mata motuhake(m2/g):40
Te ahua: Ma ki te kowhai te paura
Znic oxide Ihirangi: min 90%
Te whakarewa taimaha hei Pb2+ (%): 0.001 Max.
Te parahi hei Cu2+ (%): 0.0005 Max.
Konupora hei Mn2+ (%): 0.001 Max.
Kiato(g/mm3):3.6
Horahanga mata motuhake(m2/g):40
Te ahua: Ma ki te kowhai te paura
Znic oxide Ihirangi: min 40%
Te whakarewa taimaha hei Pb2+ (%): 0.002 Max.
Te parahi hei Cu2+ (%): 0.001 Max.
Konupora hei Mn2+ (%): 0.001 Max.