Ponagalo: Phofo ye tšhweu go ya go ye serolane
Znic oxide Diteng:88-93%
Tšhipi ye boima bjalo ka Pb2+ (%): 0.001 Max.
Koporo bjalo ka Cu2 + (%): 0.0005 Max.
Manganese bjalo ka Mn2 + (%): 0.001 Max.
Kitlano (g / mm3): 4.6
Sebaka se itseng bokagodimo(m2 / g):40
Ponagalo: Phofo ye tšhweu go ya go ye serolane
Znic oxide Diteng:min 90%
Tšhipi ye boima bjalo ka Pb2+ (%): 0.001 Max.
Koporo bjalo ka Cu2 + (%): 0.0005 Max.
Manganese bjalo ka Mn2 + (%): 0.001 Max.
Kitlano (g / mm3): 3.6
Sebaka se itseng bokagodimo(m2 / g):40
Ponagalo: Phofo ye tšhweu go ya go ye serolane
Znic oxide Diteng:min 40%
Tšhipi ye boima bjalo ka Pb2+ (%): 0.002 Max.
Koporo bjalo ka Cu2 + (%): 0.001 Max.
Manganese bjalo ka Mn2 + (%): 0.001 Max.